Substituted 3, 4-polymethylenedioxythiophenes, and polymers and electro responsive devices made therefrom ML Blohm, JE Pickett, PC VanDort US Patent 5,111,327, 1992 | 165 | 1992 |
Hydrolysis kinetics of condensation polymers under humidity aging conditions JE Pickett, DJ Coyle Polymer Degradation and Stability 98 (7), 1311-1320, 2013 | 113 | 2013 |
Photodegradation of UV screeners JE Pickett, JE Moore Polymer Degradation and Stability 42 (3), 231-244, 1993 | 103 | 1993 |
Effects of irradiation conditions on the weathering of engineering thermoplastics JE Pickett, DA Gibson, MM Gardner Polymer Degradation and Stability 93 (8), 1597-1606, 2008 | 96 | 2008 |
Sample temperatures during outdoor and laboratory weathering exposures JE Pickett, JR Sargent Polymer Degradation and Stability 94 (2), 189-195, 2009 | 74 | 2009 |
Synthesis, characterization, and stability of poly (3, 4-dibutoxythiophenevinylene) copolymers ML Blohm, JE Pickett, PC Van Dort Macromolecules 26 (11), 2704-2710, 1993 | 71 | 1993 |
Fluoride-promoted, dye-sensitized photooxidation of enols HH Wasserman, JE Pickett Journal of the American Chemical Society 104 (17), 4695-4696, 1982 | 70 | 1982 |
Effects of temperature on the weathering of engineering thermoplastics JE Pickett, DA Gibson, ST Rice, MM Gardner Polymer Degradation and Stability 93 (3), 684-691, 2008 | 63 | 2008 |
The fluoride ion effect in the reactions of singlet oxygen with enols HH Wasserman, JE Pickett Tetrahedron 41 (11), 2155-2162, 1985 | 56 | 1985 |
High‐throughput fabrication, performance testing, and characterization of one‐dimensional libraries of polymeric compositions RA Potyrailo, RJ Wroczynski, JE Pickett, M Rubinsztajn Macromolecular rapid communications 24 (1), 123-130, 2003 | 53 | 2003 |
Life prediction for CIGS solar modules part 2: degradation kinetics, accelerated testing, and encapsulant effects DJ Coyle, HA Blaydes, RS Northey, JE Pickett, KR Nagarkar, RA Zhao, ... Progress in Photovoltaics: Research and Applications 21 (2), 173-186, 2013 | 45 | 2013 |
Review and kinetic analysis of the photodegradation of UV absorbers JE Pickett Macromolecular symposia 115 (1), 127-141, 1997 | 44 | 1997 |
High‐Throughput Multilevel Performance Screening of Advanced Materials RA Potyrailo, JE Pickett Angewandte Chemie International Edition 41 (22), 4230-4233, 2002 | 42 | 2002 |
Service life prediction of polymers and plastics exposed to outdoor weathering C White, KM White, J Pickett William Andrew, 2017 | 38 | 2017 |
Weathering of plastics JE Pickett Handbook of environmental degradation of materials, 163-184, 2018 | 37 | 2018 |
Influence of photo-Fries reaction products on the photodegradation of bisphenol-A polycarbonate JE Pickett Polymer degradation and stability 96 (12), 2253-2265, 2011 | 37 | 2011 |
Global weathering of aromatic engineering thermoplastics JE Pickett, MM Gardner, DA Gibson, ST Rice Polymer degradation and stability 90 (3), 405-417, 2005 | 37 | 2005 |
The dye-sensitized photooxidation of imidazoles: trapping of intermediates by nucleophiles HH Wasserman, MS Wolff, K Stiller, I Saito, JE Pickett Tetrahedron 37, 191-200, 1981 | 31 | 1981 |
Highly predictive accelerated weathering of engineering thermoplastics JE Pickett, V Umamaheswaran SAE transactions, 689-693, 2003 | 30 | 2003 |
Photostability of UV screeners in polymers and coatings JE Pickett, JE Moore | 30* | 1996 |